Product Name | Hastelloy B-3 Bar/Rod | |
Technology | Hot rolled , Cold rolled | |
Grade | Inconel 600, Inconel 601, Inconel 625, Inconel 617, Inconel 690, Inconel 718, Inconel X-750 | |
Incoloy A-286, Incoloy 800, Incoloy 800H, Incoloy 800HT Incoloy 825, Incoloy 901, Incoloy 925, Incoloy 926 | ||
Monel 400, Monel K-500 | ||
Hastelloy X,Hastelloy C22 ,Hastelloy C-276, Hastelloy B-2, Hastelloy B-3 | ||
Specifications | ASTM, UNS, JIS, EU | |
Surface | 2B, 2D, BA, NO.1, NO.4, NO.8, 8K, mirror, checkered, embossed, hair line, sand blast, Brush, etching, etc | |
Shape | Rod, Round, Channel Bar, Rings, Round Rod, Triangle, Hollow, Rectangle, T-Bar, Flat Bar, Precision Ground Bar, Blocks, Square, Threaded, Hex (A/F), Profiles, Half Round Bar, Ingot, Billet, I/H Bar, Forging etc. | |
Processing Service | Machining : Turning / Milling / Planing / Drilling / Boring / Grinding / Gear Cutting / CNC Machining Deformation processing : Bending / Cutting / Rolling / Stamping | |
Delivery time | 10-30 days subject to the clients' requirement and quantity | |
Package | clients' requirement and Standard export sea-worthy packing | |
MOQ | 1 ton |
Available Size Range
Dimension | Range |
Diameter | 3、5、6、7、8、9、10、12、15、18、20、25、30、35、40、50、100、200 etc |
Length | 1000mm, 2500mm, 3000mm,3500mm, 4000mm 5000mm 6000mm 10000mm 12000mm, etc or as customer's request |
Chemical Analysis (%)
Alloy | C | Si | Mn | P | S | Cr | Ni | Co | Mo | W | Al | Ti | Cu | V | Fe |
Hastelloy B-3 | ≤0.01 | ≤0.10 | ≤3.00 | ≤0.03 | ≤0.01 | 1.0-3.0 | ≥65.0 | ≤3.00 | 27.0-32.0 | ≤3.00 | ≤0.50 | ≤0.20 | ≤0.20 | ≤0.20 | 1.0-3.0 |
About Hastelloy B-3
Hastelloy B-3 is a nickel-molybdenum alloy with excellent resistance to hydrochloric acid at all concentrations and temperatures. It also withstands sulfuric, acetic, formic and phosphoric acids, and other nonoxidizing media. B-3 alloy has a special chemistry designed to achieve greater thermal stability than B-2 alloy, resulting in easier fabrication.
Because this alloy contains no significant chromium addition it should NOT be used in oxidizing media or in presence of oxidizing salts, such as ferric or cupric salts. The latter may form when iron or copper is present in a system containing hydrochloric acid. Likewise alloy B-3 does not withstand wet chlorine gas or hypochlorite bleach.